| C core |  | | | Material
Using 0.23mm、0.27mm、0.30mm、0.35mm Low iron loss high permeability cold-rolled orientation of high quality silicon steel materials
FEATURES
As it is a structure of two split half combing a closed magnetic circuit, it s an open form, the coil production can be separated from the core production, then put the wound coils onto the core, production period would be shortened.
Application range
Widely used in electromagnetic components in electroninc equipoment such as transformer,current transformer, reactor etc. | |  |
|
|